Salt-damaged render and plaster repair
Repairing render, plaster and mortar damaged by salt damp in Melbourne buildings: salt removal, lime or sacrificial plasters, repointing and published costs.
Salt-damaged render and plaster repair removes finishes that have been broken down by salts carried up the wall by damp, deals with the salts left in the masonry, and refinishes the wall with materials that let it keep drying. Doing it before the moisture source is fixed wastes money, because new plaster on a wet, salty wall breaks down the same way. Through this site, enquiries go to independent providers who quote the repair and do the work.

Why does plaster keep failing at the base of the wall?
Heritage Victoria’s flood-affected masonry technical note explains the process. Moisture carrying soluble salts soaks into porous brick, stone and mortar. When the water evaporates the salt stays behind as tiny crystals, and over repeated wet and dry cycles those crystals build enough pressure to push the grains of the material apart. The note calls this salt attack and describes it as the main way masonry decays in older buildings.
The salts concentrate where the wall dries fastest. If that point is in your plaster, the plaster crumbles. If a hard render or cement repair stops drying at the surface, the salts move into the brick or mortar behind it instead.
What are the signs?
- Plaster that sounds hollow when tapped, bulges or falls away near the floor
- Paint lifting in blisters with white powder behind it
- Fluffy or crusty white crystals on brick, render or plaster
- Mortar joints eroded back from the face of the bricks at the base of outside walls
- Damage that appears above a cement-rendered plinth on the outside of the house
Repair options compared
| Option | What it is | When it suits | What to know |
|---|---|---|---|
| Strip and leave to dry | Remove failed plaster back to masonry and let the wall dry before refinishing | Every job, after the moisture source is fixed | Drying can take months on thick walls |
| Captive-head washing | Low-pressure water spray inside an enclosed head, with the salty water vacuumed back | Walls with smaller salt loads | Several passes may be needed in one day |
| Poulticing | Absorbent paper-pulp mix applied wet, left to dry and peeled off with the salt | Walls with heavy salt loads | Each cycle takes weeks, at least two cycles |
| Sacrificial plaster or mortar | Deliberately weak, porous lime mix that takes the salt damage instead of the wall | Follow-up after washing or poulticing | Will need replacing over time |
| Lime plaster or render | Breathable finish suited to older masonry | Heritage and pre-war walls | Different trade skills from gypsum plastering |
| Cement render or gypsum plaster | Harder, less permeable finishes | Modern masonry where suitable | The heritage note warns against these on old salt-affected walls |
The washing and poulticing methods, cycle times and the warning about cement and gypsum all come from the heritage note. It also says not to remove original lime plasters that are still sound, and to replaster with lime-based materials rather than gypsum.
What does a provider need to know?
- Whether the moisture source has been found and fixed, ideally with a rising damp inspection report
- The area of plaster or render affected, room by room and on each outside wall
- Whether the walls were originally lime plaster, and whether earlier repairs used cement
- Any heritage listing that affects external render or paint
- Whether decorative features such as cornices or ceiling roses need protecting
What does the repair involve?
- Protect floors and remove skirting boards.
- Strip loose and salt-damaged plaster to sound material, usually to a line above the highest damage.
- Rake out hard cement repairs from mortar joints. The heritage note describes cutting along the centre of the joint with a small diamond disc, then chiselling the mortar out towards the cut so brick edges are not damaged.
- Extract salts by washing or poulticing, measuring progress with a conductivity meter where the job warrants it.
- Repoint with a mortar weaker and more porous than the bricks, which for older walls means a lime mortar, as the heritage note recommends.
- Apply sacrificial or lime plaster, let it cure, then finish with a breathable paint.
How much does it cost?
These published Melbourne ranges cover the parts of the job most often quoted separately:
| Item | Published Melbourne range |
|---|---|
| Old render removal | $14 to $36 per sqm |
| Cement render, applied | $27 to $54 per sqm |
| Plaster skim coat | $16 to $52 per sqm |
| Plaster water damage repair | $315 to $1,575 |
| Brick pointing or repointing | $42 to $160 per sqm |
The render and plaster tables do not price lime work, salt extraction or poulticing separately, so expect those to be quoted per job. The rising damp cost guide shows how these items combine with the damp-proofing work.
Rules that apply
If the outside of the building is in a Heritage Overlay, re-rendering or repainting can require council approval. According to the City of Melbourne’s heritage overlay guidance, a permit is needed to externally paint a heritage place where the schedule sets paint controls, and to externally alter the building. The BPC registration threshold for domestic building work counts the whole project, so a large combined damp-proofing and re-plastering job may need a registered builder.
What a careful provider will refuse to do
- Re-plaster before the moisture source is dealt with
- Use waterproof paint, sealers or hard renders to cover salts, which the heritage note says trap moisture and salt in the wall
- Paint previously unpainted heritage brick with anything other than a traditional limewash
- Remove sound original lime plaster to make the job uniform
Local angle
These repairs come up most in inner Melbourne’s older terrace streets, where much of the housing was built with lime mortar and plaster before cement took over after the Second World War. Our pages on Fitzroy and Melbourne cover the building types there, and damp-proof course injection explains the barrier work that often comes first.
What to do next
Get a plaster and render repair quote by listing the rooms and walls affected, whether a damp-proof course has been installed or repaired, and whether the building is heritage listed. Photos of the worst areas and the outside face of the same walls help.
Frequently asked questions
- Why does new plaster keep blowing off the wall?
Salts left in the masonry dissolve and recrystallise as humidity changes. If the moisture source is still active or the salts were not removed, new plaster breaks down in the same zone. Fix the source, remove salts, then replaster with a suitable material.
- Can I paint over salt stains?
Painting hides the stain for a short time. Waterproof paints and sealers trap moisture and salt in the wall and can move the damage into the brick or mortar. Use a breathable finish once the wall has dried.
- Is lime plaster necessary?
For older walls built with lime mortar and plaster, Heritage Victoria recommends lime-based materials rather than gypsum. For modern masonry, the provider may suggest other finishes suited to the wall.
- How is salt removed from a wall?
Two common methods are captive-head washing, which sprays and vacuums water across the surface, and poulticing, which uses an absorbent paste that dries and is peeled away with the salt. Sacrificial plasters can then catch deeper salts over time.
- Do I need a permit to re-render the front of my house?
If the house is in a Heritage Overlay, external alterations and in some cases external painting need a planning permit. Check the overlay schedule for your address before booking the work.